![](/img/cover-not-exists.png)
Pitting corrosion of carbon steel caused by iron bacteria
David Starosvetsky, Robert Armon, Josef Yahalom, Jeana StarosvetskyVolume:
47
Year:
2001
Language:
english
Pages:
9
DOI:
10.1016/s0964-8305(99)00081-5
File:
PDF, 650 KB
english, 2001