In-situ laser ultrasonic grain size measurement in superalloy INCONEL 718
Garcin, Thomas, Schmitt, Jean Hubert, Militzer, MatthiasLanguage:
english
Journal:
Journal of Alloys and Compounds
DOI:
10.1016/j.jallcom.2016.01.222
Date:
February, 2016
File:
PDF, 5.47 MB