![](/img/cover-not-exists.png)
The effects of cold rolling orientation and water chemistry on stress corrosion cracking behavior of 316L stainless steel in simulated PWR water environments
Chen, Junjie, Lu, Zhanpeng, Xiao, Qian, Ru, Xiangkun, Han, Guangdong, Chen, Zhen, Zhou, Bangxin, Shoji, TetsuoVolume:
472
Language:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2016.01.018
Date:
April, 2016
File:
PDF, 4.57 MB
english, 2016