Nanoindentation of closed cell Al alloy foams subjected to different heat treatment regimes
Šnajdar Musa, Mateja, Marić, Gojko, Grilec, KrešimirVolume:
89
Language:
english
Journal:
Composites Part B: Engineering
DOI:
10.1016/j.compositesb.2013.12.079
Date:
March, 2016