Fabrication strain rate-stress corrosion property correlations of thermomechanically treated 15Cr-15Ni-2-2Mo titanium modified austenitic stainless steel
Shaikh, H., Sivaprasad, P. V., Vinoy, T. V., Bharathi, G., Venkadesan, S., Khatak, H. S.Volume:
14
Language:
english
Journal:
Materials Science and Technology
DOI:
10.1179/mst.1998.14.11.1175
Date:
November, 1998
File:
PDF, 1.98 MB
english, 1998