![](/img/cover-not-exists.png)
Kinetic study by differential scanning calorimetry of the bulk copolymerization of 2-hydroxyethylmethacrylate with ethyleneglycoldimethacrylate
N. Ajzenberg, A. RicardVolume:
80
Year:
2001
Language:
english
Pages:
9
DOI:
10.1002/app.1207
File:
PDF, 222 KB
english, 2001