![](/img/cover-not-exists.png)
Tuning the mechanical properties of vertical graphene sheets through atomic layer deposition
Davami, Keivan, Jiang, Yijie, Cortes, John, Lin, Chen, Shaygan, Mehrdad, Turner, Kevin T, Bargatin, IgorVolume:
27
Language:
english
Journal:
Nanotechnology
DOI:
10.1088/0957-4484/27/15/155701
Date:
April, 2016
File:
PDF, 1.32 MB
english, 2016