Quantitative fractography by digital image processing: NIH Image macro tools for stereo pair analysis and 3-D reconstruction
L. R. O. HeinVolume:
204
Year:
2001
Language:
english
Pages:
12
DOI:
10.1046/j.1365-2818.2001.00920.x
File:
PDF, 8.03 MB