Development of NIMS burner rig and cyclic testing of nickel base superalloys
Matsumoto, K, Koizumi, Y, Kawagishi, K, Harada, HVolume:
50
Language:
english
Journal:
Canadian Metallurgical Quarterly
DOI:
10.1179/1879139511Y.0000000011
Date:
July, 2011
File:
PDF, 393 KB
english, 2011