Influences of niobium and solution treatment temperature on pitting corrosion behaviour of stabilised austenitic stainless steels
Bai, Guanshun, Lu, Shanping, Li, Dianzhong, Li, YiyiLanguage:
english
Journal:
Corrosion Science
DOI:
10.1016/j.corsci.2016.03.009
Date:
March, 2016