Characterization of epoxy prepreg SPX 8800 system by isothermal differential scanning calorimetry
Wang, Qian, Storm, Birgit K.Volume:
193
Journal:
Macromolecular Symposia
DOI:
10.1002/masy.200390068
Date:
March, 2003
File:
PDF, 832 KB
2003