![](/img/cover-not-exists.png)
Influence of tempering treatment on microstructure and pitting corrosion resistance of a new super ferritic–martensitic–austenitic stainless steels with 17%Cr
Pardal, J. M., da Silva, M. R., Bastos, I. N., de Macêdo, M. C. S., Tavares, S. S. M.Language:
english
Journal:
Corrosion Engineering, Science and Technology
DOI:
10.1080/1478422x.2015.1110418
Date:
April, 2016
File:
PDF, 1.13 MB
english, 2016