![](/img/cover-not-exists.png)
Damage Resistance of a Thermal Barrier Coated Superalloy for Combustor Liners in Aero Turbines During Fatigue and Creep
Ray, Ashok K., Goswami, B., Kar, A., Ray, Ajoy K., Das, H.K., Roy, P.K., Kumar, S.B., Bose, S.C.Volume:
47
Journal:
Canadian Metallurgical Quarterly
DOI:
10.1179/cmq.2008.47.4.479
Date:
December, 2008
File:
PDF, 1.69 MB
2008