Durability test on coral Ce0.9Gd0.1O2-δ-La0.6Sr0.4Co0.2Fe0.8O3-δ with La0.6Sr0.4Co0.2Fe0.8O3-δ current collector working in SOFC and SOEC modes
Sar, Jaroslaw, Schefold, Josef, Brisse, Annabelle, Djurado, ElisabethVolume: