Intergranular Stress Corrosion of Stainless Steel
Carter, RalphVolume:
23
Language:
english
Journal:
Canadian Metallurgical Quarterly
DOI:
10.1179/cmq.1984.23.1.85
Date:
January, 1984
File:
PDF, 2.50 MB
english, 1984