Microstructure and Microanalysis of Ni-based Superalloy Exhaust Valves
Evans, N. D., Maziasz, P. J., Walker, L. R.Volume:
10
Language:
english
Journal:
Microscopy and Microanalysis
DOI:
10.1017/s1431927604885192
Date:
August, 2004