Micromechanical properties on the surface of PVC/SBR blends spatially resolved by a nanoindentation technique
Shui-Han Zhu, Chi-Ming Chan, Yiu-Wing MaiVolume:
44
Year:
2004
Language:
english
Pages:
6
DOI:
10.1002/pen.20055
File:
PDF, 210 KB
english, 2004