![](/img/cover-not-exists.png)
Stress corrosion behavior of T91 steel in static lead–bismuth eutectic at 480 °C
Liu, Jing, Jiang, Zhizhong, Tian, Shujian, Huang, Qunying, Liu, YuejingVolume:
468
Language:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2015.09.032
Date:
January, 2016
File:
PDF, 1.82 MB