Stress corrosion cracking of high-strength AZ31 processed by high-ratio differential speed rolling
Shi, Zhiming, Kim, W.J., Cao, Fuyong, Dargusch, Matthew S., Atrens, AndrejVolume:
3
Language:
english
Journal:
Journal of Magnesium and Alloys
DOI:
10.1016/j.jma.2015.11.006
Date:
December, 2015
File:
PDF, 4.20 MB
english, 2015