![](/img/cover-not-exists.png)
Temperature-modulated differential scanning calorimetry studies on the origin of double melting peaks in isothermally melt-crystallized poly(L-lactic acid)
Yeong-Tarng Shieh, Gin-Lung LiuVolume:
45
Year:
2007
Language:
english
Pages:
9
DOI:
10.1002/polb.21056
File:
PDF, 331 KB
english, 2007