Nanoindentation of biodegradable cellulose diacetate-graft-poly(L-lactide) copolymers: Effect of molecular composition and thermal aging on mechanical properties
Seung-Hwan Lee, Yoshikuni Teramoto, Siqun Wang, George M. Pharr, Timothy G. RialsVolume:
45
Year:
2007
Language:
english
Pages:
8
DOI:
10.1002/polb.21074