![](/img/cover-not-exists.png)
Ballistic transport and reaction modeling of atomic layer deposition manufacturing processes
Adomaitis, Raymond AVolume:
44
Language:
english
Journal:
IFAC Proceedings Volumes
DOI:
10.3182/20110828-6-it-1002.02276
Date:
January, 2011
File:
PDF, 778 KB
english, 2011