![](/img/cover-not-exists.png)
A positron annihilation study of rotating beam fatigue damage in the superalloy Haynes 188
D. Hoeckelman, H. P. Leighly Jr.Volume:
149
Year:
1995
Language:
english
Pages:
1
DOI:
10.1002/pssa.2211490232
File:
PDF, 281 KB
english, 1995