Nanoporous Membranes Produced from Polycrystalline Ni-Based Superalloys
Schmitz, Fabian, Rösler, JoachimVolume:
10
Language:
english
Journal:
Journal of Nanoscience and Nanotechnology
DOI:
10.1166/jnn.2010.2586
Date:
September, 2010