![](/img/cover-not-exists.png)
Surface analysis of plasma-treated polydimethylsiloxane by x-ray photoelectron spectroscopy and surface voltage decay
Bok-Hee Youn, Chang-Su HuhVolume:
35
Year:
2003
Language:
english
Pages:
5
DOI:
10.1002/sia.1558
File:
PDF, 322 KB
english, 2003