Oxidative stability of camelina (Camelina sativaL.) oil using pressure differential scanning calorimetry and Rancimat method
Ratusz, Katarzyna, Popis, Edyta, Ciemniewska-Żytkiewicz, Hanna, Wroniak, MałgorzataVolume:
126
Language:
english
Journal:
Journal of Thermal Analysis and Calorimetry
DOI:
10.1007/s10973-016-5642-0
Date:
October, 2016
File:
PDF, 623 KB
english, 2016