![](/img/cover-not-exists.png)
A Single-Crystal Co-Base Superalloy Strengthened by γ′ Precipitates: Structure and Mechanical Properties
Petrushin, Nikolay, Hvatzkiy, Konstantin, Gerasimov, Victor, Link, Thomas, Epishin, Alexander, Nolze, Gert, Gerstein, GregoryVolume:
17
Language:
english
Journal:
Advanced Engineering Materials
DOI:
10.1002/adem.201500088
Date:
June, 2015
File:
PDF, 2.17 MB
english, 2015