Effect of Water Impurities on Stress Corrosion Cracking in a Boiling Water Reactor
Ljungberg, Lars G., Cubicciotti, DanielVolume:
41
Language:
english
Journal:
Corrosion
DOI:
10.5006/1.3582006
Date:
May, 1985
File:
PDF, 2.70 MB
english, 1985