Mechanical and Microstructural Investigation of Nickel-Based Superalloy IN718 Manufactured by Selective Laser Melting (SLM)
Strößner, Johannes, Terock, Michael, Glatzel, UweVolume:
17
Language:
english
Journal:
Advanced Engineering Materials
DOI:
10.1002/adem.201500158
Date:
August, 2015
File:
PDF, 1.50 MB
english, 2015