![](/img/cover-not-exists.png)
Fractographic Aspects of the Stress Corrosion Cracking of Titanium in a Methanol/HCl Mixture
SPURRIER, J., SCULLY, J. C.Volume:
28
Journal:
Corrosion
DOI:
10.5006/0010-9312-28.12.453
Date:
December, 1972
File:
PDF, 12.68 MB
1972