Mechanical properties of bamboo fiber cell walls during the culm development by nanoindentation
Huang, Yanhui, Fei, Benhua, Wei, Penglian, Zhao, ChangVolume:
92
Language:
english
Journal:
Industrial Crops and Products
DOI:
10.1016/j.indcrop.2016.07.037
Date:
December, 2016