Microstructural evolution and pitting corrosion behavior of...

Microstructural evolution and pitting corrosion behavior of friction stir welded joint of high nitrogen stainless steel

Zhang, H., Wang, D., Xue, P., Wu, L.H., Ni, D.R., Ma, Z.Y.