Effect of three-stage homogenization on mechanical properties and stress corrosion cracking of Al-Zn-Mg-Zr alloys
Xiao, Tao, Deng, Yunlai, Ye, Lingying, Lin, Huaqiang, Shan, Chaojun, Qian, PengweiVolume:
675
Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2016.08.071
Date:
October, 2016
File:
PDF, 8.47 MB