![](/img/cover-not-exists.png)
Effect of Grain Size on Stress Corrosion of Type 302 Austenitic Stainless Steel
BARNWELL, V. L, MYERS, J. R., SAXER, R. K.Volume:
22
Journal:
CORROSION
DOI:
10.5006/0010-9312-22.9.261
Date:
September, 1966
File:
PDF, 770 KB
1966