![](/img/cover-not-exists.png)
Thermomechanical processing of a nickel-base superalloy powder compact
Kandeil, A.Y., Immarigeon, J-P.A., Wallace, W., de Malherbe, M.C.Volume:
1
Language:
english
Journal:
High Temperature Technology
DOI:
10.1080/02619180.1983.11753209
Date:
May, 1983
File:
PDF, 4.87 MB
english, 1983