8th International Symposium on Superalloy 718 and Derivatives (Ott/8th International) || Finite Element Analysis Using a Dislocation Density Based Flow Stress Model Coupled with Model for Precipitate Evolution
Ott, Eric, Banik, Anthony, Andersson, Joel, Dempster, Ian, Gabb, Tim, Groh, Jon, Heck, Karl, Helmink, Randy, Liu, Xingbo, Wusatowska-Sarnek, AgnieszkaVolume:
10.1002/97
Year:
2014
Language:
english
DOI:
10.1002/9781119016854.ch13