![](/img/cover-not-exists.png)
Effect of isothermal annealing of amorphous alloys on their tendency toward pitting corrosion
Yu. A. Pustov, Yu. V. Baldokin, V. Yu. Vasil'ey, V. N. Shumilov, A. N. KlochkoVolume:
28
Language:
english
Pages:
6
DOI:
10.1007/bf00707101
Date:
November, 1986
File:
PDF, 557 KB
english, 1986