Peridynamical Modelling of Nanoindentation in Ceramic Composites
Sadowski, Tomasz, Pankowski, BłażejVolume:
254
Language:
english
Journal:
Solid State Phenomena
DOI:
10.4028/www.scientific.net/SSP.254.55