Mechanical properties of UO2 thin films under heavy ion irradiation using nanoindentation and finite element modeling
Elbakhshwan, Mohamed S., Miao, Yinbin, Stubbins, James F., Heuser, Brent J.Volume:
479
Language:
english
Journal:
Journal of Nuclear Materials
DOI:
10.1016/j.jnucmat.2016.07.047
Date:
October, 2016
File:
PDF, 3.18 MB
english, 2016