![](/img/cover-not-exists.png)
Variation of transitional functions in multiscale fatigue crack growth of superalloys
Tang, K.K., Berto, F., Wu, H.Volume:
2
Year:
2016
Language:
english
Journal:
Procedia Structural Integrity
DOI:
10.1016/j.prostr.2016.06.236
File:
PDF, 656 KB
english, 2016