Hydrophobic surface treatment and interrupted atomic layer deposition for highly-resistive Al2O3 films on graphene
Jeon, Jae Ho, Jerng, Sahng-Kyoon, Akbar, Kamran, Chun, Seung-HyunLanguage:
english
Journal:
ACS Applied Materials & Interfaces
DOI:
10.1021/acsami.6b09531
Date:
October, 2016
File:
PDF, 1.11 MB
english, 2016