International Journal of Materials Research (formerly Zeitschrift fuer Metallkunde)
2015 / 07 Vol. 106; Iss. 7
![](/img/cover-not-exists.png)
Dynamic precipitation of nickel-based superalloys undergoing severe deformation below the solvus temperature
Nowotnik, Andrzej, Rokicki, Paweł, Mrówka-Nowotnik, Grażyna, Sieniawski, JanVolume:
106
Language:
english
Journal:
International Journal of Materials Research
DOI:
10.3139/146.111263
Date:
July, 2015
File:
PDF, 4.09 MB
english, 2015