![](/img/cover-not-exists.png)
Fractography and X-ray photoelectron spectroscopy of free-machining steels
Doyle, E. D., Aghan, R. L., Larkins, F. P., Hughes, M. E.Volume:
13
Language:
english
Journal:
Metal Science
DOI:
10.1179/030634579790434105
Date:
October, 1979
File:
PDF, 2.07 MB
english, 1979