![](/img/cover-not-exists.png)
Microstructural and Creep Properties of Boron- and Zirconium-Containing Cobalt-based Superalloys
Bocchini, Peter J., Sudbrack, Chantal K., Noebe, Ronald D., Dunand, David C., Seidman, David N.Language:
english
Journal:
Materials Science and Engineering: A
DOI:
10.1016/j.msea.2016.10.124
Date:
November, 2016
File:
PDF, 1.79 MB
english, 2016