Creep-fatigue life prediction and interaction diagram in nickel-based GH4169 superalloy at 650 °C based on cycle-by-cycle concept

Wang, Run-Zi, Zhang, Xian-Cheng, Gong, Jian-Guo, Zhu, Xu-Min, Tu, Shan-Tung, Zhang, Cheng-Cheng