![](/img/cover-not-exists.png)
Non-isothermal crystallization kinetics of Ga–Sn–Te chalcogenide glasses by differential scanning calorimetry
Zhang, Yaqi, Li, Pengfei, Gao, Peng, Tu, Wenkang, Wang, Li-MinVolume:
52
Language:
english
Journal:
Journal of Materials Science
DOI:
10.1007/s10853-016-0586-0
Date:
March, 2017
File:
PDF, 1.94 MB