![](/img/cover-not-exists.png)
Creep Crack Initiation and Growth Behavior for Ni-Base Superalloys
NAGUMO, Yoshiko, YOKOBORI, Jr., A. Toshimitsu, SUGIURA, Ryuji, OZEKI, Go, MATSUZAKI, TakashiVolume:
6
Year:
2012
Language:
english
Journal:
Journal of Solid Mechanics and Materials Engineering
DOI:
10.1299/jmmp.6.610
File:
PDF, 4.89 MB
english, 2012