Monte Carlo Simulation Taking Account of Surface Crack Effect for Stress Corrosion Cracking in a Stainless Steel SUS 304
TOHGO, Keiichiro, SUZUKI, Hiromitsu, SHIMAMURA, Yoshinobu, NAKAYAMA, Guen, HIRANO, TakashiVolume:
74
Year:
2008
Journal:
Transactions of the Japan Society of Mechanical Engineers Series A
DOI:
10.1299/kikaia.74.128