Recognition of Internal Weld Defects by Defect Model.
Ishii, Akira, Lachkhia, Vakhtang, Ochi, Yasuo, Akutsu, MasayukiVolume:
60
Year:
1994
Journal:
Transactions of the Japan Society of Mechanical Engineers Series A
DOI:
10.1299/kikaia.60.2440