![](/img/cover-not-exists.png)
Surface analysis of cements after having been immersed in water - Surface state and elementary analysis of zinc phosphate cement and carboxylate cement.
KIKUCHI, Hisaji, HIROSE, Hideharu, IDE, Ryuzo, SEMI, Seisuke, KAWAKAMI, Tatsumi, MATSUKURA, Kazuo, ANZAI, Misaki, OHASHI, MasayoshiVolume:
25
Year:
1983
Language:
english
Journal:
The Journal of Nihon University School of Dentistry
DOI:
10.2334/josnusd1959.25.277
File:
PDF, 1.17 MB
english, 1983